Customization: | Available |
---|---|
Type: | Rolling Wire |
Material: | Nickel / Nickel Alloy |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
ERNiCrCo-4 Product Description
Material Type: Nickel-Chromium-Cobalt-Molybdenum Superalloy
AWS Specification: AWS A5.14
Key Characteristics
1. Chemical Composition (Typical):
Nickel (Ni): Base element (≥50%), ensuring strength and resilience.
Chromium (Cr): 20-23% (enhances oxidation resistance), vital for longevity.
Cobalt (Co): 10-15% (improves high-temperature stability), perfect for demanding environments.
Molybdenum (Mo): 8-10% (resists localized corrosion), boosting durability.
Iron (Fe): ≤5%, a controlled element for balance.
Exceptional resistance to pitting, crevice corrosion, and stress corrosion cracking (SCC) in the most challenging acidic, alkaline, and chloride-rich environments, such as marine and chemical processing.
Mechanical Strength:
Outstanding tensile strength (≥750 MPa) paired with excellent creep resistance, ensuring reliability even under prolonged high-temperature stress.
Weldability:
Seamlessly compatible with GTAW (TIG), GMAW (MIG), and SMAW processes, ensuring versatile application.
Minimal post-weld cracking due to its low carbon content, enhances structural integrity and longevity.
Product Forms & Specifications
Available Forms:
Welding consumables: Available as wire (0.8-4.0 mm diameter) and electrodes to meet diverse needs.
Mill products: Offered in round bars, sheets, plates, and coils for various industrial applications.
Standards: Complies with ASTM B574 and AMS 5826 (if applicable) to guarantee quality and reliability.
Packaging: Welding wires are sealed in moisture-proof packaging; bulk materials are standard crated for protection.
Applications
Aerospace: Ideal for combustion chambers, turbine blades, and exhaust systems, offering unmatched performance.
Energy: Essential for *** core components and heat exchangers, providing resilience and safety.
Oil & Gas: Perfect for downhole tools, valves, and piping in sour gas environments, ensuring robustness.
Chemical Processing: Designed for reactors, scrubbers, and piping used with sulfuric acid, hydrochloric acid, and seawater, providing superior resistance.
Processing & Fabrication
Machining: Employ carbide tools with low cutting speeds and ample coolant for precision and efficiency.
Heat Treatment: Solution annealing at 1120-1175°C followed by rapid quenching for optimal performance.
Welding Notes:
Preheat is unnecessary for thin sections, simplifying procedures.
Post-weld heat treatment (PWHT) is optional for critical applications, providing flexibility.
________________________________________
Notes
1. Cobalt (Co) Role: Cobalt enhances high-temperature strength and reduces thermal expansion, making ERNiCrCo-4 suitable for ultra-high-temperature environments, a hallmark of quality.
2. Verification Required: Confirm exact composition and certification (e.g., EN, UNS, or proprietary grades) with suppliers to ensure authenticity and suitability.
3. Alternatives: If unavailable, ERNiCrMo-4 (AWS A5.14 ERNiCrMo-4) or Inconel 617 (Ni-Cr-Co-Mo) may serve as substitutes, maintaining excellence.
AWS A5.4 | ERNi-1 | ERNiCu-7 | ERNiCr-3 | ERNiCrFe-5 | ERNiCrMo-3 | ERNiCrMo-4 | ERNiCrMo-7 |
TS(N/mm2) | 460 | 541 | 671 | 560 | 790 | 729 | 780 |
EL(%) | 30 | 39 | 39 | 30 | 43 | 33 | 35 |
C | 0.02 | 0.02 | 0.03 | 0.03 | 0.0037 | 0.002 | 0.05 |
Mn | 0.3 | 1.7 | 3.05 | 1 | 0.03 | 0.12 | 0.6 |
Si | 0.16 | 0.44 | 0.37 | 0.04 | 0.029 | 0.07 | 0.02 |
P | 0.0012 | 0.007 | / | 0.004 | 0.003 | 0.003 | 0.003 |
Ti | 2.3 | / | 0.01 | / | 0.088 | / | / |
S | 0.005 | 0.008 | / | 0.002 | 0.001 | 0.0015 | |
Cr | / | / | 19.86 | 15.7 | 21.95 | 15.9 | 16.7 |
Ni | 96.5 | 65.68 | 72.8 | 75.06 | 64.65 | REM | REM |
Cu | / | REM | 0.06 | 0.03 | 0.009 | 0.008 | / |
Mo | / | / | / | 0.03 | 9.04 | 15.9 | 15.8 |
Nb | / | / | 2.4 | 2.3 | 3.61 | / | / |
V | / | / | / | / | / | 0.01 | / |
Fe | / | 0.7 | 0.23 | 7.9 | 0.19 | 4.12 | 2.2 |