Customization: | Available |
---|---|
Type: | Rolling Wire |
Material: | Nickel / Nickel Alloy |
Still deciding? Get samples of $ !
Order Sample
|
Shipping Cost: | Contact the supplier about freight and estimated delivery time. |
---|
Payment Methods: |
![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() |
---|---|
Support payments in USD |
Secure payments: | Every payment you make on Made-in-China.com is protected by the platform. |
---|
Refund policy: | Claim a refund if your order doesn't ship, is missing, or arrives with product issues. |
---|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
AWS A5.14: ERNiCrMo-13
UNS Number: W86113 (Weld Metal), N06059 (Solid Wire)
Typical Composition (% wt.):
Ni: Balance (~59%)
Cr: 22.0-24.0%
Mo: 15.0-16.5% (Higher than ERNiCrMo-10)
Fe: ≤1.0% (Very low)
Co: ≤0.3%, Mn: ≤0.5%, Si: ≤0.1%
C: ≤0.010% (Ultra-low carbon)
Impurities (S/P): ≤0.015%
Primarily used for:
UNS N06200 (Alloy 59)
UNS N06022 (Alloy C-22)
UNS N10276 (Alloy C-276)
Also welds dissimilar combinations (e.g., Ni-alloys to stainless steels).
Critical Metrics:
PREN (Pitting Resistance Equivalent): >75 (Higher than ERNiCrMo-10).
CPT/CCT: Exceeds Alloy C-276/C-22.
Property | Value |
---|---|
Tensile Strength | 115-125 ksi (790-860 MPa) |
Yield Strength | 60-70 ksi (415-480 MPa) |
Elongation | 35-45% |
Impact Toughness | >75 J @ -196°C |
Density: 8.6 g/cm³
Melting Range: 1310-1350°C (2390-2460°F)
Thermal Expansion: 13.5 μm/m·°C (20-100°C)
Chemical Processing: Reactors, piping, and scrubbers handling sulfuric/hydrochloric acids.
Pollution Control: Flue gas scrubbers (FGD), waste incineration systems.
Pharmaceutical: Equipment exposed to aggressive sterilants (e.g., hypochlorite).
Marine: Seawater-cooled heat exchangers, offshore piping.
Processes: GTAW (TIG), GMAW (MIG).
Shielding Gas:
GTAW: Argon or Ar + He (≤50% He).
GMAW: Ar + He + ≤1% CO2.
Heat Input: Low (≤1.2 kJ/mm) to avoid segregation.
Preheat/Interpass: ≤100°C (212°F) - avoid overheating.
AWS A5.4 | ERNi-1 | ERNiCu-7 | ERNiCr-3 | ERNiCrFe-5 | ERNiCrMo-3 | ERNiCrMo-4 | ERNiFeCr-1 |
Tensile Strength (N/mm2) |
514 | 541 | 671 | 651 | 819 | 729 | 602 |
Elongation (%) |
44 | 39 | 41 | 45 | 39 | 45 | 33 |
C | 0.02 | 0.02 | 0.03 | 0.06 | 0.037 | 0.012 | 0.02 |
Mn | 0.24 | 3.21 | 3.05 | 0.51 | 0.06 | 0.5 | 0.5 |
Si | 0.34 | 0.68 | 0.12 | 0.14 | 0.11 | 0.01 | 0.11 |
P | 0.34 | 1.53 | 2.4 | 1.99 | 3.37 | 0.23 | 0.81 |
Ti | 0.34 | 1.53 | / | / | / | / | 0.81 |
S | 0.14 | 0.47 | 1.41 | 6.82 | 3.9 | 5.4 | 28.24 |
Cr | / | / | 19.86 | 14.79 | 21.55 | 15.9 | 22.61 |
Ni | 95.5 | 65.68 | 72.8 | 75.06 | 61.65 | REM | 42.91 |
Cu | 0.01 | REM | 0.03 | 0.03 | / | / | / |
Mo | 0.01 | REM | 0.03 | 0.03 | 8.49 | 16 | 2.67 |
Nb | / | 2.4 | 1.99 | 3.37 | / | ||
V | / | 0.23 | |||||
Fe | 0.14 | 0.47 | 1.41 | 6.82 | 3.9 | 5.4 | 28.24 |